Datasheets give times per developer, dilution and temperature, usually at 20 °C. "Stock" means the developer as mixed; "1+9" means one part developer to nine parts water. More dilute developer works slower, so times get longer.
Temperature matters a lot: warmer developer works faster. Kodak's tables for Tri-X give times from 18 to 24 °C.
Longer development raises contrast and density; that is how pushing and pulling work. Starting from the datasheet and adjusting to your own results is normal practice.
Every film page on rolllog lists the times its datasheet gives, and the developer pages list every film for one developer.